Yes. With the HILCO Aluminil electrodes, you weld aluminium with an ordinary electrode welding machine, without shielding gas and without a gas cylinder. For gas welding, there are also cored rods with an internal flux, which do not require a separate flux.
Why this is practical
MIG and TIG welding of aluminium requires a gas cylinder, a wire feeder and a suitable power source. For a repair in the field or on board a ship, that equipment is often not available. With a covered aluminium electrode, you only need a power source and an electrode holder. That makes emergency repairs to aluminium components possible on site as well.
The range
Product Classification Intended for Aluminil Si5 EN ISO 18273 E Al 4043 Pure aluminium and AlMgSi alloys Aluminil Si12 EN ISO 18273 E Al 4047 AlSi casting alloys up to 12 percent silicon Fluxcored AlSi5 Cored rod Gas welding and surfacing, flux in the core Fluxcored Al99.5 Cored rod Gas welding of pure aluminium Aluminil Si12 has been developed specifically for welding AlSi casting alloys. The high silicon content improves the flow characteristics of the weld pool and reduces crack sensitivity. The colour of the weld metal closely matches aluminium castings, which matters for visible repairs.
Points of attention when welding
- Clean the surface thoroughly, aluminium quickly forms an oxide layer
- Store the electrodes dry, the special coating limits moisture absorption but does not rule it out
- Take the high thermal conductivity of aluminium into account when setting your machine
- When TIG welding, use the right tungsten electrode, which you can find among the accessories
Typical repairs
The Aluminil electrodes are used for engine blocks, cylinder heads, pump housings, machine beds and components in the maritime sector. They are products for repair work, not for series production. For production welding of aluminium, MIG or TIG remains the preferred route.
The electrodes are supplied in hermetically sealed aluminium tins, packed six to an outer box. This packaging keeps the product dry until the moment of use.
What you can expect
A covered aluminium electrode is a repair solution. The weld metal is soft and ductile with good mechanical properties, and the corrosion resistance is good. For production work, long continuous welds and structures with high requirements for appearance, MIG or TIG remains the preferred route.
Bear in mind that aluminium dissipates heat quickly. With thicker components, preheating is required to achieve good fusion. With thin parts, the risk is precisely that of burn-through, because aluminium does not change colour when heated and you therefore have little visual warning.
We are happy to think along with you about the approach to an aluminium repair.